Factory dope

Posted: Mon Jul 27, 2015 01:27
by skyking3286
Factory applied fabric that already had one coat on it as they applied it. So they only sprayed two coats! And the lightweight cotton was only expected to be on for ten years at the most.

Re: Factory dope

Posted: Mon Jul 27, 2015 17:16
by Paul Agaliotis
Mark,
They also used hot dope for the covering. It's no wonder there were so many dope room explosions.
Paul

Re: Factory dope

Posted: Thu Jul 30, 2015 00:43
by Captgrumps
Average recover was 4-5 years depending on where it sat and what area (mostly outdoors)--labor was cheap then and so were the Aeronca's..

Re: Factory dope

Posted: Thu Jul 30, 2015 00:48
by Paul Agaliotis
Doug,
How it has changed. Now the most expensive part of the cover job is the labor.